Dimensional stability of iron at high temperature
| |
GRAY IRON |
DUCTILE IRON |
LOW CARBON STEEL CASTING |
LOW ALLOY STEEL CASTING |
| 1 |
Shape stability |
Excellent |
Average |
Bad |
Average |
| 2 |
Creep, (%/hr at 8000F, 25 Ksi) |
Excellent .001-.01 |
Average .02-.20 |
Bad / Average .05-.5 |
Good .005-.05 |
| 3 |
Resistance to swelling |
Bad |
Good |
Good / Very good |
Very good
|
|